A shop in Johor was making spiral duct for a data centre job. Monday's sections passed the visual check and the water test. Thursday's sections had porosity along the seam, and the client's inspector stopped the delivery. Nothing on the line had been changed, or so everyone said. It turned out the operator on the night shift had raised the wire feed speed by a small amount to reduce spatter, and had not written it down. Two shifts, one machine, two different welds, and no record connecting either to a setting.
That is a version-control problem, not a welding problem. The machine was fine. The knowledge about how to run it was not pinned down. Over the years I have come to treat the weld parameter sheet as a controlled document, the same way an aircraft maintenance manual is controlled. It sounds heavy for a duct shop. In practice it is a one-page sheet and a pencil.
This article is about how I set up those sheets, how I stop them drifting, and what to put on them. It applies to spiral seam welding, to the spot welds on a round pipe line, and to the tack welds used before flange attachment.
A useful sheet is short. If it runs to three pages, nobody will use it at the machine. Mine fits on one A4 sheet and covers one joint type. The fields below are the ones that have earned their place; everything else has been tried and removed.
Current in amps, arc voltage, wire feed speed, travel speed, gas flow in litres per minute, electrode extension, and polarity. On a resistance spot welder the equivalent fields are weld current, squeeze time, weld time, hold time and electrode force. Write the units next to every number, because "60" means nothing on its own and I have seen it read as amps by one shift and as litres by another.
Include the range, not just the centre value. "Voltage 18–19 V" tells the operator where the acceptable window is. A single number implies that any deviation is a fault, which is not how a welding process actually behaves, and it encourages people to hide small adjustments rather than record them.
Material grade and thickness, coating type and weight, joint preparation, fit-up gap, and the position of the weld. On galvanised sheet the coating changes everything: a Z275 coil needs different treatment from Z100, and the sheet should say which one the parameters were developed on. If the coil changes and the sheet does not, the sheet is already out of date.
I also record the consumable: wire diameter and type, gas mixture, and the electrode or tip type on a spot welder. A change of wire spool from one supplier to another is a process change even when the label looks identical.
One line describing what a correct weld looks like, and one describing the common defect if the drift goes the wrong way. For a spiral seam: "continuous bead, no undercut, uniform ripple; porosity indicates gas or zinc issue." This gives the operator something to compare against without needing a metallurgy degree.
Parameters drift for predictable reasons. An operator makes a small adjustment to solve a immediate problem — more heat to burn through a dirty edge, less current to stop burn-through on a thin coil. The adjustment works. It stays. The next shift inherits it as the new normal. Six weeks later nobody remembers the original setting, and the sheet on the wall describes a process that no longer exists.
The fix is a revision log that lives on the same sheet. Every change gets a number, a date, a short reason, and a name. Not a signature in blood — a first name is enough. The point is to make a change visible and to make the reason recoverable.
| Rev | Date | Change | Reason | By |
|---|---|---|---|---|
| 0 | 12 Mar | Initial settings, 1.2 mm Z275 | FAT baseline | Chen |
| 1 | 04 Apr | Wire feed 5.2 → 5.6 m/min | Lack of fusion on doubler joint | Ravi |
| 2 | 19 May | Gas 14 → 16 L/min | Porosity on night shift, fan draught | Chen |
| 3 | 02 Jul | Travel speed −8% | New operator, bead too narrow | Siti |
| 4 | 21 Aug | Reverted to rev 2 for Z100 only | Coating change, burn-through | Chen |
Look at rev 3. "New operator, bead too narrow" is an odd reason to change a machine parameter, and that is exactly the kind of entry a log should surface. The correct response to a new operator is training, not a process change. A log that nobody reads will not catch this; a supervisor who glances at it during a weekly walk will.
I keep old revisions in a folder, not in the bin. When a defect appears, the first question is always "when did it start," and the revision log answers that in seconds. On the Johor job, a four-line log would have shown the wire feed change on the same day somebody noticed the porosity.
This is the detail that trips up most first attempts. A line makes many joints: the longitudinal spiral seam, the tack welds at the flange, the spot welds on a round pipe, the repair weld on a damaged panel. Each has its own parameter set. If you write one sheet for the whole machine, it will be wrong for at least half the work.
Name the sheet by the joint, not by the operator or the shift. "Spiral seam, 0.8–1.2 mm galvanised" and "Spot weld, 1.0 mm, two thicknesses" are good names. Put a code on it — SS-01, SW-02 — and refer to that code in the work order. When a batch is rejected six months later, the code tells you exactly which parameters were in force.
Material thickness ranges need care. A single sheet covering 0.8 to 1.2 mm is acceptable if the window is broad enough for both; it is not acceptable if the operator has to guess where in the range a particular coil sits. Where the difference matters, split the sheet. I would rather have four short sheets than one ambiguous one. The spiral forming machine page describes the seam arrangement; use it to decide how many distinct joints your line actually produces.
Everyone can propose a change. Nobody should be able to make one silently. In a small shop the rule can be as simple as "operators use the sheet; the supervisor signs a revision." In a shop with a quality system, route revisions through whoever owns the weld procedure. The exact hierarchy matters less than the fact that there is one.
I give experienced operators a bounded window. Within the printed range they may adjust freely and note the value on the production record. Going outside the range requires a revision. This respects the fact that a good operator reads the weld and adjusts for a draughty door or a slightly oxidised coil, while still keeping the process inside a known envelope.
One useful trick: print the allowed range in a coloured band on the sheet. Green is the normal window, amber means "adjust and tell someone," red means stop. People understand colour faster than text at 5 a.m., and a glance is enough to see whether a machine is being run outside its envelope.
A parameter sheet and a first-off inspection are two halves of the same control. The sheet says what the machine should be doing; the first-off check says what it actually did. Keep them together. I put a small box at the bottom of the sheet for the first-off result — date, operator, visual pass or fail, and any measurement taken.
On a resistance welder the useful measurement is a peel test on a sample coupon made from the same two thicknesses. Pull it apart and look at the button size. A spot weld that looks fine on the surface can have a nugget half the diameter it should. I ask for one coupon at the start of each shift and whenever the coil changes; that takes ninety seconds and catches drift before it becomes a batch problem.
For seam welds, a water test or an air test on the first finished section is the practical check. If the section fails, do not adjust the machine and immediately make another. Write down what you changed, then make the next section. The temptation to fix and re-test without recording is the single biggest source of undocumented process drift I encounter.
The machine page for the round pipe spot welder gives the electrode arrangement; use it when you write the sheet for that station, because electrode wear changes the effective current density even when the dial has not moved.
A new operator should be trained against the same document they will use on the line. Sit them at the machine with the sheet, point to each field, and ask them to set the values from scratch. Then deliberately introduce a fault — a gas line half closed, a wire spool of the wrong diameter — and see whether they notice. People learn a parameter sheet far faster when they have had to defend it once.
Keep a second copy in the training folder and use the revision log as the training record. When rev 2 was signed off, everyone working on that joint should have seen it. A quick signature next to the revision number in the folder is enough, and it removes the argument about whether a change was communicated.
Where language is an issue, photograph the actual machine dials with the correct settings marked and put the photos on the sheet. I did this on a line in Vietnam where the operators were comfortable with the machine but not with the English terms. A picture of the gas regulator at 16 litres was worth more than a paragraph of text.
Keep one master copy of each sheet in an office folder, either paper or a simple scanned PDF. Keep a printed copy at the machine, laminated if the environment is oily. When a revision is issued, remove the old copy from the machine — do not leave it there "for reference." Two versions on the wall is how the wrong one gets used.
Name the files so they sort sensibly: joint code, revision, date. A folder containing "weld final v2 REALLY FINAL.pdf" is not a controlled document system. It is a cry for help. I have seen that exact filename in a shop that failed a customer audit over it.
Finally, tie the sheets into the broader machine documentation. The cutting station has its own settings and consumables, and the habit of recording changes at the weld station tends to spread once one area is disciplined. Start with the joint that causes the most rework. Once that sheet is trusted, the rest follow without much persuasion.
Not for ordinary HVAC duct in most markets, but you do need a documented, repeatable setting and evidence that the joint passes its test. A controlled parameter sheet plus first-off records satisfies that for commercial work. If the client specifies a code — pressure duct, cleanroom, or a certified project — follow their qualification requirement and treat your sheet as the shop-level translation of it.
At every coil or consumable change, every six months as a routine, and immediately after any weld defect that is not obviously explained. The review is a ten-minute conversation, not a rewrite. Most revisions I approve are a single number moving slightly inside a range, recorded so the next shift knows it happened.
One named person, usually the production supervisor or the quality lead. That person issues revisions and removes old copies from the machine. If nobody owns the folder, the system decays within a month — I have watched it happen several times, and it always starts with an unlabelled photocopy pinned next to the original.
Yes, provided they record what they changed. Within the green band they are doing their job: reading the weld and compensating for real conditions. Outside it, they stop and call someone. A rule that forbids all adjustment is unrealistic and drives the practice underground, which is worse than a small documented variation.